Rutile: How to Process This Titanium Ore?
A rutile concentrate with 90% TiO 2 and a garnet and omphacite concentrate with a purity of 88% are obtained. The recovery rates of the three minerals are all above 67%. 2. Processing rutile from heavy mineral sands. Take the Sierra Leone rutile processing plant as …